Oxide Sublimation during the High-temperature Oxidation of Nickel Alloys with Protective Coatings
03.09.2008 г.

Oxide Sublimation during the High-temperature Oxidation

of Nickel Alloys with Protective Coatings

E. G. Ivanov

Zhukovskii Air Force Academy

e-mail: Этот e-mail защищен от спам-ботов. Для его просмотра в вашем браузере должна быть включена поддержка Java-script

Received October 16, 2006

Abstract — It is shown that the oxidation of heat-resistant alloys is accompanied by a sublimation of the oxides MoO3, WO3, Al2O3, and CrO3. The determinant in the sublimate is the molybdenum content, exceeding that in scale by a factor of 50–100. Protective coatings diminish the sublimation, rather than fully eliminate it. To diminish the molybdenum oxide sublimation decisively, it is expedient to alloy the coating with magnesium or magnesium oxide.

PACS numbers: 81.65.Kn

 

DOI: 10.1134/S0033173208040139